You start a print, walk away, and come back to a tangle of plastic spaghetti and a part dragged across the bed. Or a corner lifted halfway through and the whole thing failed. Prints not sticking to the bed is the most common 3D printing problem there is, and the good news is that the most effective fixes cost nothing. This guide goes through them in the order that solves the problem fastest.

Why won't my print stick to the bed?

Most prints come loose because the plate is greasy or the first layer is not pressed onto it firmly enough. Everything else, from temperature to drafts, matters less often.

A 3D print holds onto the bed only through its first layer. That layer has to be melted plastic squashed onto a clean, warm surface so it grips. Anything that gets between the plastic and the plate, like a fingerprint, weakens the grip, and anything that keeps the line from being pressed down, like a nozzle set a fraction too high, leaves it sitting loosely on top. As the part grows and cools, it pulls on that first layer, and a weak spot lets go.

Eight fixes for prints not sticking, in order: wash the plate with dish soap, wipe with 90% isopropyl alcohol, recalibrate the first layer, use the filament's bed temperature, match the plate to the filament, slow the first layer, block drafts or use an enclosure, replace a worn plate
The first three fixes are free and solve most cases. Image: PrintStock

1. Clean the plate the right way

Wash the plate with warm water and a little dish soap when adhesion drops, and wipe it with strong isopropyl alcohol between prints. This single habit fixes more failed prints than any setting.

Prusa's support guides recommend isopropyl alcohol (IPA) of 90% or stronger as the everyday degreaser, and a wash with a few drops of dish soap in warm, not hot, water when adhesion keeps decreasing even with IPA. The reason is simple: alcohol dissolves light grease but tends to spread heavier skin oil around, while soap lifts it off. Use plain dish soap, not hand soap, which can leave moisturiser behind. Rinse well, dry with a clean paper towel, and hold the plate by its edges from then on.

Two cautions from the same guides: never use acetone on a textured powder-coated sheet, and do not clean PETG off a sheet with IPA right before printing PETG again, because IPA can make PETG bond extremely strongly.

2. Get the first layer right

The first layer must be squashed slightly onto the plate: too high and the lines do not bond, too low and the nozzle scrapes and blocks. This distance is called the Z offset.

Look at the first layer as it prints. Good lines are flat, slightly wider than the nozzle and merge into a smooth, even surface. Round, separate lines that you can see gaps between mean the nozzle is too high. Thin, transparent or rough, scraped lines mean it is too low. Most modern printers measure the bed automatically, but the offset between the nozzle and the sensor can drift after a nozzle swap, a plate change or a knock. Run your printer's first layer calibration, or adjust the offset in small steps while watching a test square.

Other first-layer settings help too: print the first layer slower, which gives the plastic more time to bond, and slightly hotter, and turn the part cooling fan off or low for it. Your printer maker's profile usually already does this.

3. Use the right bed temperature

Set the bed to the temperature on your filament's data sheet. As examples, Prusa's data sheets give 40 to 60 °C for its PLA and about 80 °C for its PETG, and Bambu Lab gives 80 to 100 °C for its ABS.

Too cold and the plastic does not grip; too hot, especially with PLA, and the bottom of the part stays soft, which causes "elephant's foot" bulging and can actually reduce grip on some plates. If you changed filament brand and adhesion got worse, check that the bed temperature in your profile matches the new spool.

4. Match the plate to the filament

Different plates suit different materials, and the wrong pairing either will not stick or sticks too well. Most owners need only one plate for everyday printing.

Build plate types: textured PEI for everyday printing and easy release; smooth PEI for glossy bottoms, needs glue with PETG; cool or low-temperature plates for PLA at low bed temperatures; engineering plates for nylon and polycarbonate with glue
Most people need one textured plate; the others solve specific materials and finishes. Image: PrintStock

Textured PEI is the easiest everyday surface: it grips PLA, PETG, ABS and TPU when hot and releases them when cool. Smooth PEI gives a glossy bottom face but can bond too strongly with PETG; Prusa advises against printing PETG on smooth PEI without glue as a release layer. Low-temperature "cool" plates help PLA stick with little heat, and engineering plates with glue are for nylon and polycarbonate. Check which plates fit your printer before buying; size and alignment pins differ.

5. Slow down and help small parts

A slower first layer, a brim and fewer tall thin parts all help prints stay down. They matter most for models with a small footprint.

A tall, thin part with a tiny base has very little first layer to hold it and a lot of leverage to pull it off. A brim, a flat ring of extra plastic around the base, adds contact area and peels off afterwards. Mouse ears, small discs at sharp corners, do the same for corners that lift. Orienting the model so its largest flat face sits on the bed is often the simplest fix of all.

6. Block drafts and keep the part warm

Drafts cool one side of a print faster than the other, and the shrinking plastic pulls corners off the bed. This is the main cause of warping with ABS and ASA, and it affects large PLA parts too.

Keep the printer away from open windows, fans and air conditioning vents. For ABS and ASA, an enclosure that keeps the whole part warm is close to essential. Our guide to PLA vs PETG vs ABS explains which materials need one.

7. Check for a worn plate

If a clean plate on a calibrated printer still loses grip, the plate is probably worn out. PEI surfaces are a consumable: Prusa notes that PEI can lose its adhesion after a couple of hundred hours of printing.

Signs of a worn plate are shiny, smooth patches where you print most, scratches and gouges from tools, coating that is peeling, and a plate that is bent so the first layer is uneven. Replacing a plate is cheap compared with hours of failed prints. Here are the printers in our catalog whose owners report first-layer or adhesion problems as a known issue, so you can see whether yours is one of them:

Owners report this on 41 of the 370 printers we track

And 29 more; see each printer page.

Is it the printer or me?

Almost always, adhesion problems are fixable at home without a new printer. It is a frustrating problem because it feels random, but it follows a short list of causes.

If you have worked through cleaning, first layer calibration and bed temperature and prints still come loose only in one area of the bed, the bed may be uneven or the automatic levelling may need re-running. If they come loose only with one filament, the plate and temperature are the suspects. If they come loose only on tall or narrow parts, it is geometry, and a brim fixes it.

Common mistakes

The most common mistake is reaching for glue or hairspray before cleaning the plate properly. They hide the problem for a few prints and add a layer that needs cleaning off.

  • Touching the plate after cleaning it. One fingerprint undoes the wash.
  • Using weak alcohol. 70% rubbing alcohol leaves water and additives behind; use 90% or stronger.
  • Using acetone on a textured plate. It can damage the coating.
  • Scraping parts off with a metal blade. It gouges the coating and creates the next adhesion problem.
  • Printing PETG on smooth PEI without glue. It can tear the coating when you remove the part.