You print a box that should slide into a slot, and it will not go in. Look at the bottom: the first few layers flare outward like the foot of an elephant. It is one of the most common first-layer flaws, it ruins fits and dimensions, and it is easy to fix once you know which knob causes it.
What is elephant's foot in 3D printing?
Elephant's foot is a bulge at the bottom of a print, where the first layer or the first few layers are wider than the rest of the part. The walls go straight up, except at the base, which flares out by a fraction of a millimetre.

It is easy to confuse with two other base problems:
- Warping lifts the corners off the plate. The base is bent upward, not wider. See print warping.
- A squashed first layer looks thin, see-through or scraped, sometimes with ridges. It is often the same root cause as elephant's foot, seen from below.
Elephant's foot is mostly invisible on decorative prints. It matters on parts that must fit: boxes with lids, holes for screws or bearings, slots, and anything that sits flush against another part.
What causes elephant's foot?
The first layer spreads wider than the model says it should. Three things make it spread, and they often act together.
- Nozzle too close to the bed. A first layer squashed hard gets pressed sideways. A slightly squashed first layer is what makes prints stick, so many printers are set on the low side on purpose.
- Bed too hot. The bottom layers stay soft, and the weight of the print presses them outward. Bambu Lab's wiki notes that the weight of the upper layers can make the first layer expand, and that the effect is usually more visible on larger models.
- Too much plastic on the first layer. A flow rate set too high, or a first-layer line width or flow boosted in the slicer for better adhesion, puts extra plastic where it can only go sideways.
There is a built-in tension here: the same squish that helps a first layer stick also causes elephant's foot. The goal is enough squish to stick, and no more.
How to fix elephant's foot, in order

Start with the settings that cause it, then let the slicer compensate for what remains.
1. Raise the nozzle slightly
Increase the first-layer gap in small steps: a Live Z or Z-offset change of about 0.02 to 0.05 mm at a time. The first layer should still be flat and fused, with lines merging into a solid sheet, but not shiny-thin or scraped. Our bed levelling guide shows what a good first layer looks like.
2. Lower the bed temperature
Try 5 to 10 °C lower, staying inside the range the filament maker publishes. Some slicers let you set a separate bed temperature for the first layer and the rest; a slightly cooler bed after the first layer helps big, heavy parts.
3. Check flow on the first layer
If you have raised the first-layer flow or line width for adhesion, set it back to the profile default. If every layer looks overfilled, calibrate flow for that filament; most slicers include a flow calibration test.
4. Turn on elephant foot compensation
Every major slicer can shrink the first layer to cancel out the spread.
- PrusaSlicer: Print Settings, Advanced, Elephant foot compensation (Advanced or Expert mode). Prusa's help article says values around 0.2 mm usually work well for a 0.4 mm nozzle, and its official profiles have it turned on.
- Bambu Studio: Process, Quality, Elephant foot compensation, per Bambu Lab's wiki. OrcaSlicer has the same setting in the same place.
- Cura: Initial Layer Horizontal Expansion, with a small negative value.
Change it in steps of about 0.05 mm and print a small test. Too much compensation makes the base undersized, and the brim stops touching the part: Prusa names this as the sign that the setting is too high. If you use a brim, keep compensation modest.
5. Design it out
If you design your own parts, add a small 45 degree chamfer, about 0.5 mm, around the bottom edge. Any leftover bulge fills the chamfer instead of sticking out. Many designers do this as a habit on parts that must fit.
Fixing it after printing
A bulge that is already there can be trimmed. Run a deburring tool or a sharp craft knife along the bottom edge, or sand it on a flat sheet of sandpaper. It is quick on small parts, tedious on many, so fix the settings for the next batch.
When the build plate is the problem
An uneven plate makes elephant's foot appear in some areas and not others. If one corner of the bed squashes the first layer harder than the rest, prints placed there bulge more. Clean the plate, re-run the printer's levelling, and replace a plate that is dented or worn: a damaged surface forces you to run the nozzle lower than you should.
Where to go from here
If your first layer will not stick once you raise the nozzle, see prints not sticking to the bed. For PETG, which needs a less squashed first layer than PLA, see our PETG settings guide.