Your print looks fragile, the walls do not quite meet, the top surface has holes, and the infill looks like a loose net. That is under-extrusion: the printer is pushing out less plastic than the slicer planned. It is one of the most common 3D printing problems, and it has a handful of usual causes. This guide shows how to recognise it and how to track down the cause without guessing.
What is under-extrusion?
Under-extrusion is when the printer lays down less plastic than the slicer planned, so lines are thinner than they should be and do not fuse properly. The result is gaps, weak bonds between lines and layers, and parts that break easily.
The slicer calculates exactly how much filament to push for every line, based on the nozzle size, layer height, line width and filament diameter. If less plastic actually comes out, for whatever reason, every line is thinner than planned. The printer does not know; it just keeps going, and the part comes out sparse and weak.
How to recognise under-extrusion
Look for gaps between lines, thin walls, holes in top surfaces and parts that feel light and crack easily. It may affect the whole print or appear only at times, which is itself a clue.
- Lines that do not touch each other, with visible gaps.
- Gaps between the outer walls and the infill.
- Thin, missing or broken walls.
- Holes or a mesh-like pattern on top surfaces.
- Weak layers that split apart under light force.
- A clicking extruder during the print.
Under-extrusion that appears only on fast sections, such as long straight infill lines, points to a flow limit. Under-extrusion that comes and goes points to a mechanical cause, such as a spool that drags or gears that slip. Under-extrusion only on the first layer usually means the nozzle is too close to the bed.
Under-extrusion vs over-extrusion
Under-extrusion is too little plastic; over-extrusion is too much. The fixes point in opposite directions, so it is worth being sure which one you have.
| Under-extrusion | Over-extrusion |
|---|---|---|
Lines | Thin, with gaps | Wide, merging into blobs |
Walls | Thin, sometimes missing | Bulging, rough |
Top surface | Holes, mesh pattern | Ridges, rough, nozzle drags |
Dimensions | Fine or slightly small | Too large, holes too small |
Strength | Weak, splits easily | Usually strong but ugly |
Common causes | Clog, wet filament, slipping gears, flow limit | Flow set too high, wrong filament diameter |
What causes under-extrusion, in order
Check the hardware first: nozzle, filament, extruder, then temperature and speed, and settings last. Most under-extrusion is mechanical, and changing slicer settings over a mechanical problem only hides it for a while.

1. A partial clog or a worn nozzle
A partly blocked nozzle is the most common cause. Debris or burnt plastic narrows the opening, and less plastic gets through. Clear it with heat, the cleaning needle and a cold pull, as described in our guide to a clogged nozzle. If you have printed abrasive filament through a brass or stainless nozzle, the hole may be worn and rounded, which also causes thin, inconsistent lines; replace the nozzle.
2. Wet, tangled or dragging filament
Wet filament, a tangled spool or a stiff filament path all reduce the plastic that reaches the nozzle. Wet filament also causes popping and bubbles. Dry the spool, check that it unwinds freely, and look for tight bends or kinks in any PTFE tube between the spool and the extruder. Our guide on how to dry filament covers temperatures for each material.
3. Slipping or worn extruder gears
If the extruder gears slip, the filament does not move as far as the printer thinks. You will often hear clicking and see filament with chewed marks. Clean dust and plastic shavings from the gears, check the tension arm if your extruder has one, and replace gears that are worn, which happens fast with abrasive filaments.
4. Nozzle temperature too low for the speed
At the low end of a filament's temperature range, plastic may not melt fully at higher speeds. Raise the nozzle temperature by 5 °C at a time within the maker's range and test. If you recently switched to a hardened steel nozzle, it heats a little less efficiently than brass and may need a few degrees more.
5. Printing faster than the hotend can melt
Every hotend and filament has a maximum volumetric flow, the cubic millimetres of plastic per second it can melt. Above that limit, plastic comes out under-melted and thin.
Slicers set this limit per filament. In Bambu Studio, for example, Bambu Lab's wiki notes that its TPU 95A profile allows 6.4 mm³/s while the generic TPU profile allows only 3.2 mm³/s, and its generic PETG HF profile for damp filament limits flow to 16 mm³/s with a lower temperature. If you use a generic profile, or override speeds, you can push past what the hotend can melt.

Lower the speed or the maximum volumetric flow, or fit a high-flow hotend if your printer supports one and you want to print faster.
6. Flow and filament settings
Only once the hardware is right, check the flow rate and the filament diameter in the slicer. A filament set to 2.85 mm on a 1.75 mm printer, or a flow multiplier lowered during an old experiment, under-extrudes every print. Run a flow calibration from your slicer, or use your printer's automatic flow calibration if it has one.
Which parts to check or replace
The parts behind most under-extrusion are cheap: the nozzle, the hotend, the extruder gears and the PTFE tube. These are the matching parts in our catalog, listed with the printers they fit and the prices we last checked:
| Part | Fits | From |
|---|---|---|
| AOSEED X-MAKER JOY Nozzle ModuleAoseed | Aoseed X-Maker Joy | $19.99as of Nov 12, 2026 |
| 0.4 mm Hotend Kit for Centauri 2 Series/Centauri Carbon 2 Series (2pcs)Elegoo | Elegoo Centauri Carbon 2 | $29.99as of Nov 11, 2026 |
| AOSEED X-MAKER Extruder ModuleAoseed | Aoseed X-Maker | $9.99as of Nov 12, 2026 |
| Creality × Phaetus Silicon Carbide Nozzle 0.4/0.6 mmCreality | Creality K2, Creality K2 Pro, Creality K2 Plus | $27.71as of Nov 11, 2026 |
| Artillery M1 Ceramic Heater and ThermistorArtillery | Artillery M1 Pro, Artillery M1 Pro S1 | $16.99as of Nov 12, 2026 |
| Artillery M1 Toolhead Extruder AssemblyArtillery | Artillery M1 Pro, Artillery M1 Pro S1 | $39.99as of Nov 12, 2026 |
| Flashforge AD5X Nozzle AssemblyFlashforge | Flashforge AD5X | $25as of Nov 12, 2026 |
| Bambu High Flow Hotend - Bambu Lab H3CBambu Lab | Bambu Lab H3C | $59.99as of Nov 11, 2026 |
| Assembled Extruder Kit for Neptune 4 ProElegoo | Elegoo Neptune 4 Pro | $43.99as of Nov 11, 2026 |
| FLSUN S1 Pro Hardened Steel Nozzles (5 pcs)FLSUN | FLSUN S1 Pro | $36.99as of Nov 12, 2026 |
| Ender-5 Max Ceramic Heating Block KitCreality | Creality Ender-5 Max | $24.99as of Nov 11, 2026 |
| Creality Ender-3 V3 SE Print Head KitCreality | Creality Ender-3 V3 SE | $8.84as of Nov 12, 2026 |
Live from our catalog. Open a part for every compatible printer and all prices.
Some printers have extrusion problems as a known pattern in owner reports. Here are the models in our catalog where owners report under-extrusion or extruder issues:
Owners report this on 44 of the 370 printers we track
- 3Doodler Flow: Jamming and clogging
- Anycubic Kobra 2 Neo: Single-gear extruder slips
- Anycubic Kobra 3 Max V2: ACE Pro false clog warnings (11518); PTFE tubes wear out; Open frame limits ABS and soft TPU
- Anycubic Kobra 3 V2: ACE Pro feed errors 11518 and 11519; Filament fragments block the path after color changes; Wear parts in the extruder; TPU and filled filaments not supported in the ACE Pro
- Anycubic Kobra S1 (ACE 2 Pro): ACE Pro filament jams (11518, 11511, 11519); Spool squeak and feed noise
- Anycubic Kobra S1 Max: ACE 2 Pro feeding errors
- Anycubic Photon Mono M7 Pro: Auto-fill pump tube cracks and leaks resin; Auto-feeder and purifier cannot run together
- Bambu Lab A1: AMS lite fails to feed or load filament; Toolhead screws work loose; "Failed to extrude" errors from the filament sensor
- Bambu Lab A1 mini: Toolhead screws work loose
- Bambu Lab A2L: Prints with ironing fail
- Bambu Lab H2C: TPU printing problems; Servo extruder overload
- Bambu Lab H2D: TPU clogs and oozes
And 32 more; see each printer page.
Common mistakes
The most common mistake is raising the flow rate to cover a mechanical problem. It hides a clog or slipping gears for a few prints, then the problem returns worse.
- Changing several settings at once. You will not know which change mattered.
- Ignoring wet filament. It mimics under-extrusion and no setting fixes it.
- Forcing a cleaning needle. A needle that is too thick widens the nozzle.
- Using generic filament profiles at full speed. Their flow limits are set for a reason.
- Assuming the first layer is under-extruded. Usually the nozzle is just too close.
Where to go from here
If clicking and thin lines started suddenly, start with unclogging the nozzle. If lines are thin and stringy at the same time, the filament is probably wet: see how to dry filament. For worn parts, browse nozzles, hotends and extruders for your printer in our catalog.
Printing PETG? Check that your temperatures sit inside the maker's window in our PETG settings guide.