PA Nylon Powder-coated Print Sheet
Sheet with a coating made for printing nylon (PA) without glue.
Compatibility
Fits: Original Prusa MK4S, Prusa CORE One+, Original Prusa MK4, Original Prusa i3 MK3S+
Different printer? The same build plate for other models:
- Prusa CORE One L+: CORE One L HighTemp Print Sheet
- Prusa CORE One L+: CORE One L PA Nylon Powder-coated Print Sheet
- Prusa CORE One L+: CORE One L Smooth PEI Print Sheet
- Prusa Pro HT90: HT90 HighTemp Powder-coated Print Sheet
- Prusa Pro HT90: HT90 Satin Powder-coated Print Sheet
- Prusa Pro HT90: HT90 Textured Powder-coated Print Sheet
Where to buy
Prices as of Nov 11, 2026Taxes, shipping and any import duties are worked out by the store at checkout and depend on your country; ask the store if in doubt.
Store links may be affiliate links: we may earn a commission, and it does not change your price. Affiliate disclosure
Price check
Lowest now: $54.99 (Standard).
We have tracked this price since Nov 11, 2026; 30 and 90 day lows appear here once we have that much history.
Install, limits and lifespan
- Made by
- The printer maker (official part)
Specs
- Surface
- Powder coat for nylon (PA)
- Type
- FDM build plate
- Role
- Add-on
- Printer max bed temperature
- 120 °C
What a build plate does
The build surface decides how well the first layer sticks and how the bottom of the print looks. Textured PEI hides marks and releases easily; smooth PEI gives a glossy bottom; cool plates help PLA stick with little heat.
Problems it can help with
Owner-reported issues on the printers this part fits. A new part fixes them only when the old part is the cause.
- Original Prusa MK4S: Inconsistent first layers from load cell calibration
The MK4S keeps the MK4's load cell probing. A minority of owners report first layer problems that clear up after recalibration, cleaning the nozzle tip or replacing the load cell under warranty.
- Original Prusa MK4: Inconsistent first layers from a faulty load cell
Most owners report perfect first layers, but threads on Prusa's forum describe units whose first layer was never right until the load cell was replaced. Prusa's load cell troubleshooting guide covers calibration and checks.
- Original Prusa MK4S: First layer too low on stock settings
A firmware issue reports the MK4S first layer coming out too low with default settings.
- Original Prusa MK4S: Pricier than CoreXY rivals
The bed slinger costs more than faster enclosed CoreXY printers.
How to install or replace it
Time: 1 minute.
- Let the bed cool.
- Lift the old plate off the magnetic base.
- Place the new plate against the alignment pins or rear edge.
- Tell the printer or slicer which plate type is fitted, then print a first-layer test.
Follow the maker's own guide for your exact model; screw sizes and cable routing differ between machines. Details from Prusa Research's official product page.
When it is time for one
- Prints no longer stick even after cleaning
- Scratches, gouges or worn patches where you print most
- Prints stick so hard they tear the coating
- You want a different finish or a material the current plate does not handle
Care
Wash the plate with warm water and dish soap, wipe with IPA between prints, and never scrape it with a metal blade.
Read the full care guideFAQ
Which printers does the PA Nylon Powder-coated Print Sheet fit?
Original Prusa MK4S, Prusa CORE One+, Original Prusa MK4, Original Prusa i3 MK3S+.
How long does it take to fit a build plate?
About 1 minute. Follow the maker's own guide for your exact model; screw sizes and cable routing differ between machines.
Textured or smooth PEI?
Textured is the easy everyday choice: good grip when hot, easy release when cool. Smooth gives a shiny bottom face but needs more care with PETG, which can bond too strongly.
Why do I need glue on some plates?
PETG and TPU can bond too strongly to smooth PEI, and some engineering filaments need help to stick; a thin glue layer works as a release or adhesion aid depending on the material.